Shenzhen Bluewind Vermiculite Products Co., Ltd. sales01@bluewindvp.com 86-0755-83251674
Einzelheiten zum Produkt
Herkunftsort: Shenzhen, China
Markenname: Bluewind
Modellnummer: BWV-Leitblech
Zahlungs- und Versandbedingungen
Min Bestellmenge: 50 Stücke
Preis: $35.00/pieces 50-399 pieces
Verpackung Informationen: Freie Palette der Räucherung mit der einwickelnden und Gurtfasten Stretchfolie;
Lieferzeit: 15workdays
Versorgungsmaterial-Fähigkeit: 8000 Stück/Stück pro Monat
Shape: |
Plate |
Material: |
Vermiculite, Silver vermiculite |
SiO2 Content (%): |
45% |
Al2O3 Content (%): |
14% |
MgO Content (%): |
24% |
CaO Content (%): |
2% |
Refractoriness (Degree): |
Common (1580°< Refractoriness< 1770°) |
CrO Content (%): |
0 |
SiC Content (%): |
0 |
Processing Service: |
Cutting, Moulding |
Size: |
1200 x 1000 mm |
Thickness: |
20 mm |
Density: |
700 kgs/m³ |
Advantage: |
Lightweight |
Application: |
Wood stoves and fireplaces |
Feature: |
Thermal shock resistant |
Packing: |
Plywood Pallet |
Heat Conductivity: |
0.18-0.28 W/m.k |
Port: |
Shenzhen/ Tianjin |
Shape: |
Plate |
Material: |
Vermiculite, Silver vermiculite |
SiO2 Content (%): |
45% |
Al2O3 Content (%): |
14% |
MgO Content (%): |
24% |
CaO Content (%): |
2% |
Refractoriness (Degree): |
Common (1580°< Refractoriness< 1770°) |
CrO Content (%): |
0 |
SiC Content (%): |
0 |
Processing Service: |
Cutting, Moulding |
Size: |
1200 x 1000 mm |
Thickness: |
20 mm |
Density: |
700 kgs/m³ |
Advantage: |
Lightweight |
Application: |
Wood stoves and fireplaces |
Feature: |
Thermal shock resistant |
Packing: |
Plywood Pallet |
Heat Conductivity: |
0.18-0.28 W/m.k |
Port: |
Shenzhen/ Tianjin |
|
BWV-LD
|
BWV-Baffle
|
BWV-HD
|
|||
SiO2
|
43 Prozent
|
45%
|
55%
|
|||
Al2O3
|
11%
|
12%
|
15%
|
|||
Dichte (kg/m3)
|
500
|
600 bis 800
|
1200
|
|||
Einstufungstemperatur (°C)
|
1050
|
1100
|
1200
|
|||
Kaltbrennfestigkeit (MPa)
|
2.2
|
3.8
|
9.0
|
|||
Bruchmodul (MPa)
|
1.0
|
2.6
|
5.0
|
|||
Dauerhafte lineare Veränderung (%) x 24 Stunden
|
2%
|
1%
|
1%
|
|||
Wärmeleitfähigkeit (W/m.k)
|
|
|
|
|||
400°C
|
0.13
|
0.16
|
0.25
|
|||
600°C
|
0.15
|
0.18
|
0.27
|
|||
800°C
|
0.17
|
0.20
|
0.29
|